Huangshi Shan Lixing metallurgical sheet Co., Ltd.

当前位置:Home > Tech > HOT ROLLED HOT DIP
Hr CGL Technical Process:
Coil Loading->Uncoiling->Cutting->Welding->Entry Accumulator->Heating And Deoxidization->Galvanizing->Air Cooling->Water Quenching->Thickness Detection->Air Dryer->Tension Leveler->passivation->Air Dryer->Exit Accumulator->Oiling->Cutting->Recoiling->Coil Unloading->Packing
The Furnace Heating Style:Improved Sendzimir Heating Technology
 
 
 
Line Parameters:
Hourly Output:Max.76.3t/h
Process after Coating:Tension Leveling,Passivation or Oiling
Line Speed:
Entry Section:120mpm
Process Section:80mpm
Exit section:100mpm
Production capacity:400,000tpy
Materical:low carbon steel,carbon structural steel,improved carbon structural steel
Product spec.:
Thickness range:0.5-4.0mm
Width range:800-1350mm
I.D.:φ610mm
O.D.:maxφ2000mm,minφ800mm
Coil weight:max25t